RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of MLC-9200-000
Li et al. 2005: n(e) 0.450-0.656 µm

Wavelength: µm
 (0.45 – 0.656)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n=1.5382+0.0073λ^{-2}+4.00\text{×}10^{-5}λ^{-4}$$

Comments

25 °C. Extraordinary ray (e).

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

J. Li, C. H. Wen, S. Gauza, R. Lu and S. T. Wu. Refractive indices of liquid crystals for display applications, J. Disp. Technol. 1, 51-61, 2005