RefractiveIndex.INFO Refractive index database




Optical constants of In2O3-SnO2 (Indium tin oxide, ITO)
König et al. 2014: EMA layer; n,k 0.25-1.0 µm

Wavelength: µm
 (0.25157 – 1)  

Other optical constants

n   k   logX   logY   eV


Optical constants of roughness layer (effective medium approximation (EMA) layer), thickness d=2nm, add this layer to ITO refractive index layer (setup: BK7+ITO(d=72nm)+EMA(d=2nm)), ITO purchased from Delta Technology (CG-60IN-CUV), 15-25 ohms, ITO on BK7. ITO includes a separate roughness layer (see EMA)


[CSV - comma separated]   [TXT - tab separated]   [Full database record]


T. A. F. König, P. A. Ledin, J. Kerszulis, M. A. Mahmoud; M. A. El-Sayed, J. R. Reynolds and V. V. Tsukruk. Electrically tunable plasmonic behavior of nanocube-polymer nanomaterials induced by a redox-active electrochromic polymer, ACS Nano 8, 6182-6192 (2014)
(Numerical data provided by Tobias König)

More info - wiki

Indium tin oxide (ITO), In2O3-SnO2

Other names

Tin-doped indium oxide

External links