Optical constants of In2O3-SnO2 (Indium tin oxide, ITO)
König et al. 2014: n,k 0.25-1.0 µm

Wavelength: µm
 (0.25157 – 1)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Optical constants of thin film In2O3-SnO2 (ITO, Indium tin oxide), thickness d=72nm, purchased from Delta Technology (CG-60IN-CUV), 15-25 ohms, ITO on BK7. ITO includes a separate roughness layer (see EMA)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

T. A. F. König, P. A. Ledin, J. Kerszulis, M. A. Mahmoud; M. A. El-Sayed, J. R. Reynolds and V. V. Tsukruk. Electrically tunable plasmonic behavior of nanocube-polymer nanomaterials induced by a redox-active electrochromic polymer, ACS Nano 8, 6182-6192 (2014)
(Numerical data provided by Tobias König)

More info - wiki

Indium tin oxide (ITO), In2O3-SnO2