Optical constants of GaInP (Gallium indium phosphide)
Schubert et al. 1995: n,k 0.250-0.954 µm

Wavelength: µm
 (0.24961 – 0.95395)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Ga0.51In0.49P; Eg=1.85±0.2 eV; Room temperature.

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

M. Schubert, V. Gottschalch, C. M. Herzinger, H. Yao, P. G. Snyder and J. A. Woollam. Optical constants of GaxIn1−xP lattice matched to GaAs, J. Appl. Phys. 77, 3416 (1995)

More info - wiki

Gallium indium phosphide, GaInP

Other name

Indium gallium phosphide, InGaP

External links