Optical constants of CH3NH3PbI3
Leguy et al. 2015; n,k 0.249-0.789 µm

Wavelength: µm
 (0.2490 – 0.7890)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Single crystal CH3NH3PbI3; orientation unknown; room temperature; critical point model used for fit, 249 nm - 789 nm - fit not reliable for sub-bandgap region - see reference

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

A. M. A. Leguy, Y. Hu, M. Campoy-Quiles, M. I. Alonso, O. J. Weber, P. Azarhoosh, M. van Schilfgaarde, M. T. Weller, T Bein, J. Nelson, P. Docampo, and P. R. F. Barnes. Reversible hydration of CH3NH3PbI3 in films, single crystals, and solar cells, Chem. Matter. 27, 3397-3407 (2015)