Optical constants of Au-Ag (Gold-silver alloy)
Rioux et al. 2014: n,k 0.27-1.2 µm; 70% Au 30% Ag

Wavelength: µm
 (0.270 – 1.200)  
 

Other optical constants

n   k   logX   logY   eV

Comments

70% Au, 30% Ag. Model fitted on ellipsometric measurements on five different AuAg alloy thin film compositions; Thin film compositions: Au, Au:Ag 2:1, Au:Ag 1:1, Au:Ag 1:2, Ag; Film thickness: 80 nm

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. Rioux, S. Vallières, S. Besner, P. Muñoz, E. Mazur and M. Meunier. An analytic model for the dielectric function of Au, Ag, and their alloys, Adv. Opt. Mater. 2, 176-182 (2014) (See Supporting information for MATLAB model)

More info - wiki

Gold-silver alloy, Au-Ag

Other names