Optical constants of AlON (Aluminium oxynitride, ALON)
Hartnett et al. 1998: 7.17 at.% N; n,k 0.24-5.6 µm

Wavelength: µm
 (0.24 – 5.6)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Nitrogen content: 7.17 at.%

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

T. M. Hartnett et al.. Optical properties of ALON (aluminum oxynitride), IR Phys. Technol, 39, 203-211 (1998)