Optical constants of AlON (Aluminium oxynitride, ALON)
Hartnett et al. 1998: 6.69 at.% N; n 0.24-5.6 µm

Wavelength: µm
 (0.24 – 5.6)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{2.1375λ^2}{λ^2-0.10256^2}+\frac{4.5817λ^2}{λ^2-18.868^2}$$

Comments

Nitrogen content: 6.69 at.%

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

T. M. Hartnett et al.. Optical properties of ALON (aluminum oxynitride), IR Phys. Technol, 39, 203-211 (1998)