RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of AlGaSb (Aluminium gallium antimonide)
Ferrini et al. 1998: n,k 0.207-2.480 µm; 10% Al

Wavelength: µm
 (0.207 – 2.480)  
 

Other optical constants

n   k   logX   logY   eV

Comments

AlxGa1−xSb, x = 0.1. Thin film grown by molecular beam epitaxy on a GaSb substrate.

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

R. Ferrini, M. Patrini, and S. Franchi. Optical functions from 0.02 to 6 eV of AlxGa1−xSb/GaSb epitaxial layers, J. Appl Phys. 84, 4517-4524 (1998)

More info - wiki

AlGaSb (Aluminium gallium antimonide)