Optical constants of AlGaAs (Aluminium gallium arsenide)
Aspnes et al. 1986: n,k 0.21-0.83 µm; 41.9% Al

Wavelength: µm
 (0.2066 – 0.8266)  
 

Other optical constants

n   k   logX   logY   eV

Comments

AlxGa1-xAs; x = 0.419

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. E. Aspnes, S. M. Kelso, R. A. Logan and R. Bhat. Optical properties of AlxGa1-xAs, J. Appl. Phys. 60, 754-767 (1986)

More info - wiki

Aluminium gallium arsenide, AlGaAs

Other name

Aluminum gallium arsenide