Optical constants of (C8H8)n-(C3H3N)m (Styrene-acrylonitrile, SAN)
Sultanova et al. 2009: n 0.4368-1.052 µm

Wavelength: µm
 (0.4368 – 1.052)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.3787λ^2}{λ^2-0.017842}$$

Comments

20 °C

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

N. Sultanova, S. Kasarova and I. Nikolov. Dispersion properties of optical polymers, Acta Physica Polonica A 116, 585-587 (2009)