Optical constants of C7H8 (Toluene)
Kedenburg et al. 2012: n 0.5-1.6 µm, k 0.5-1.75 µm

Wavelength: µm
 (0.5 – 1.75)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.17477λ^2}{λ^2-0.01825}$$

Comments

20 °C.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

S. Kedenburg, M. Vieweg, T. Gissibl, and H. Giessen. Linear refractive index and absorption measurements of nonlinear optical liquids in the visible and near-infrared spectral region, Opt. Mat. Express 2, 1588-1611 (2012)