Kerl and Varchmin 1995: n-Pentane; 313 K; n 0.326-0.644 µm

Wavelength: µm
 (0.326 – 0.644)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n=1.34199593-4.45661\text{×}10^{-3}λ^{-1}+4.22052\text{×}10^{-3}λ^{-2}$$

Comments

n-Pentane; 313 K (40 °C). See the original publication for the expression for n(λ,T).

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

K. Kerl, H. Varchmin. Refractive index dispersion (RID) of some liquids in the UV/VIS between 20°C and 60°C, J. Mol. Struct. 349, 257-260 (1995)