RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of CH4 (Methane)
Martonchik and Orton 1994: Solid at 30 K; n,k 0.002-100 µm

Wavelength: µm
 (0.0020 – 100.00)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Phase I solid methane at 30 K (-243.15 °C)
CAUTION: don't rely on interpolated values: Most data points represent values at local maxima or minima

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

temperature: 30 K

References

J. V. Martonchik and G. S. Orton. Optical constants of liquid and solid methane, Appl. Opt. 33, 8306-8317 (1994)

More info - wiki

Methane, CH4