Optical constants of C6H14 (Hexane)
Kozma et al. 2005: n-Hexane; n 0.230-0.6407 µm

Wavelength: µm
 (0.23 – 0.6407)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n=1.3654+3.5317\text{×}10^{-3}λ^{-2}+1.36906\text{×}10^{-5}λ^{-4}+2.3154\text{×}10^{-6}λ^{-6}$$

Comments

n-Hexane; 22 °C

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

I. Z. Kozma, P. Krok, and E. Riedle. Direct measurement of the group-velocity mismatch and derivation of the refractive-index dispersion for a variety of solvents in the ultraviolet, J. Opt. Soc. Am. B 22, 1479-1485 (2005)