RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of C2H4(OH)2 (Ethylene glycol)
Otanicar 2009: k 0.2-1.5 µm

Wavelength: µm
 (0.20 – 1.50)  
 

Other optical constants

logX   logY   eV

Comments

25 °C

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

T. P. Otanicar, P. E. Phelan J. S. Golden. Optical properties of liquids for direct absorption solar thermal energy systems, Solar Energy 83, 969-977 (2009)

More info - wiki

Ethylene glycol, C2H6O2

Chemical formula

HOCH2CH2OH

Other names

External links