Optical constants of C2H4(OH)2 (Ethylene glycol)
El-Kashef 2000: n 0.4-0.8 µm

Wavelength: µm
 (0.4 – 0.8)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n=1.386820+17856.021\text{×}10^{-6}λ^{-2}$$

Comments

20 °C

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

H. El-Kashef. The necessary requirements imposed on polar dielectric laser dye solvents, Physica B: Condensed Matter 279, 295-301 (2000)