Optical constants of C9H10O3 (Ethyl salicylate)
Rheims et al. 1997: n 0.5893-1.05 µm

Wavelength: µm
 (0.5893 – 1.05)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n=1.49376+0.00873λ^{-2}+0.00018λ^{-4}$$

Comments

20 °C

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

J. Rheims, J Köser and T Wriedt. Refractive-index measurements in the near-IR using an Abbe refractometer, Meas. Sci. Technol. 8, 601-605 (1997)