Optical constants of C6H12 (Cyclohexane)
Kozma et al. 2005: n 0.230-0.6407 µm

Wavelength: µm
 (0.23 – 0.6407)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{0.98901λ^2}{λ^2-0.01023416369}+\frac{0.01121λ^2}{λ^2-0.03623317709}$$

Comments

22 °C

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

I. Z. Kozma, P. Krok, and E. Riedle. Direct measurement of the group-velocity mismatch and derivation of the refractive-index dispersion for a variety of solvents in the ultraviolet, J. Opt. Soc. Am. B 22, 1479-1485 (2005)