RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of CCl4 (Carbon tetrachloride)
Moutzouris et al. 2013: n 0.450-1.551 µm

Wavelength: µm
 (0.45 – 1.551)  
 

Other optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.085608282+0.00053373λ^{2}+0.012201206λ^{-2}+0.000056451λ^{-4}+0.000048106λ^{-6}$$

Comments

300 K (27 °C).

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

K. Moutzouris, M. Papamichael, S. C. Betsis, I. Stavrakas, G. Hloupis and D. Triantis. Refractive, dispersive and thermo-optic properties of twelve organic solvents in the visible and near-infrared, Appl. Phys. B 116, 617-622 (2013)

More info - wiki

Carbon chloride, CCl4

Other names

External links