Optical constants of ZnSe (Zinc selenide)
Marple 1964: n 0.48-2.5 µm

Wavelength: µm
 (0.48 – 2.5)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=3.00+\frac{1.90λ^2}{λ^2-0.113}$$

Comments

Room temperature

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. T. F. Marple. Refractive index of ZnSe, ZnTe, and CdTe, J. Appl. Phys. 35, 539-542 (1964)

More info - wiki