RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of ZnO (Zinc monoxide)
Bond et al. 1965: n(e) 0.45-4.0 µm

Wavelength: µm
 (0.45 – 4)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2=2.80333+\frac{0.94470λ^{2}}{λ^2-0.3004^{2}}-0.00714λ^{2}$$

Comments

Extraordinary ray (e). Room temperature.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

1) W. L. Bond. Measurement of the refractive indices of several crystals, J. Appl. Phys. 36, 1674-1677 (1965)
2) Handbook of Optics, 3rd edition, Vol. 4. McGraw-Hill 2009
* Ref. 2 provides Sellmeier equation based on the data from ref. 1

More info - wiki

Zinc monoxide, ZnO

Other names

Zinc white, Calamine, Zinc(II) oxide, Zinc oxide.

External links