Optical constants of ZnGeP2 (Zinc germanium phosphide, ZGP)
Das et al. 2003: n(o) 1.32-11 µm

Wavelength: µm
 (1.32 – 11)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=4.67491+\frac{4.077926λ^2}{λ^2-0.159328}+\frac{1.896005λ^2}{λ^2-900}$$

Comments

Ordinary ray (o)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

S. Das et al.. Linear and nonlinear optical properties of ZnGeP2 crystal for infrared laser device applications: Revisited, Appl. Opt. 42, 4335-4340 (2003)

More info - wiki