Optical constants of YVO4 (Yttrium vanadate)
Shi et al. 2001: n(e) 0.48-1.34 µm

Wavelength: µm
 (0.48 – 1.34)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2=4.607200+\frac{0.108087}{λ^2-0.052495}-0.014305λ^{2}$$

Comments

Extraordinary ray (e)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

H. S. Shi, G. Zhang and H. Y. Shen. Measurement of principal refractive indices and the thermal refractive index coefficients of yttrium vanadate, J. Synthetic Cryst. 30, 85-88 (2001), as cited in Handbook of Optics, 3rd edition, Vol. 4. McGraw-Hill 2009