Zelmon et al. 1998: n 0.4-5.0 µm

Wavelength: µm
 (0.4 – 5)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{2.28200λ^2}{λ^2-0.01185}+\frac{3.27644λ^2}{λ^2-282.734}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. E. Zelmon, D. L. Small and R. Page. Refractive-index measurements of undoped yttrium aluminum garnet from 0.4 to 5.0 μm, Appl. Opt. 37, 4933-4935 (1998)