RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of Xe (Xenon)
Sinnock and Smith 1969: Solid at 161.35 K; n 0.3612-0.6439 µm

Wavelength: µm
 (0.3612 – 0.6439)  
 

Other optical constants

logX   logY   eV

Comments

Solid xenon at 161.35 K (-111.80 °C, melting point).

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

temperature: 161.35 K

References

A. C. Sinnock and B. L. Smith. Refractive indices of the condensed inert gases, Phys. Rev. 181, 1297-1307 (1969)

More info - wiki

Xenon, Xe

External links