Optical constants of TiO2 (Titanium dioxide)
Devore 1951: n(e) 0.43-1.53 µm

Wavelength: µm
 (0.43 – 1.53)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2=7.197+\frac{0.3322}{λ^2-0.0843}$$

Comments

Extraordinary ray (e); Room temperature

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

J. R. Devore. Refractive Indices of Rutile and Sphalerite, J. Opt. Soc. Am. 41, 416-419 (1951)

More info - wiki

Titanium dioxide, TiO2

Other names

Titanium(IV) oxide, Titania