Rakić 1998: n,k 0.2066-12.40 µm

Wavelength: µm
 (2.0664e-01 – 1.2398e+01)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Fit of the experimental data from several sources to Brendel-Bormann (BB) model

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

n_is_absolute: true
λ_is_vacuum: true

References

A. D. Rakić, A. B. Djurišic, J. M. Elazar, and M. L. Majewski. Optical properties of metallic films for vertical-cavity optoelectronic devices, Appl. Opt. 37, 5271-5283 (1998)