Optical constants of Te (Tellurium)
Caldwell and Fan 1959: n(o) 4.0-14 µm

Wavelength: µm
 (4 – 14)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=17.5346+\frac{4.3289λ^2}{λ^2-3.9810}+\frac{3.7800λ^2}{λ^2-11813}$$

Comments

Ordinary ray

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

1) R. S. Caldwell and H. Y. Fan, Optical properties of tellurium and selenium, Phys. Rev., 114, 664-675 (1959)
2) G. C. Bhar, Refractive index interpolation in phase-matching, Appl. Opt. 15, 305-307 (1976)
*Ref. 2 provides Sellmeier equation based on the data from Ref. 1

More info - wiki

Tellurium, Te

External links