Optical constants of SrF2 (Strontium fluoride)
Feldman et al. 1978: n 0.21-11.5 µm

Wavelength: µm
 (0.21 – 11.5)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{0.67805894λ^2}{λ^2-0.05628989^2}+\frac{0.37140533λ^2}{λ^2-0.10801027^2}+\frac{3.3485284λ^2}{λ^2-39.906666^2}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

A. Feldman, D. Horowitz, R. Waxier and M. Dodge. Optical materials characterization final technical report, February 1, 1978.

More info - wiki

Strontium fluoride, SrF2