Golovashkin and Motulevich 1964: n,k 0.73-12 µm; 4.2 K

Wavelength: µm
 (0.93 – 12.0)  
 

Other optical constants

n   k   logX   logY   eV

Comments

4.2 K (-269 °C)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

A. I. Golovashkin and G. P. Motulevich. Optical properties of tin at helium temperaturs, Sov. Phys. JETP 20, 44-49 (1965)