Optical constants of Sn (Tin)
Golovashkin and Motulevich 1964: n,k 0.73-12 µm; 293 K

Wavelength: µm
 (0.73 – 12)  
 

Other optical constants

n   k   logX   logY   eV

Comments

293 K (20 °C)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

A. I. Golovashkin and G. P. Motulevich. Optical and electrical properties of tin, Sov. Phys. JETP 19, 310-317 (1964)