Optical constants of SiC (Silicon carbide)
Singh et al. 1971: α-SiC; n(e) 0.488-1.064 µm

Wavelength: µm
 (0.488 – 1.064)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{5.7292λ^2}{λ^2-0.028923}$$

Comments

α-SiC (hexagonal crystal structure); Extraordinary ray (e); Room temperature.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

S. Singh, J. R. Potopowicz, L. G. Van Uitert and S. H. Wemple. Nonlinear optical properties of hexagonal silicon carbide, Appl. Phys. Lett. 19, 53 (1971)
(fit of the experimental data with Sellmeier dispersion formula: refractiveindex.info)

More info - wiki