Optical constants of Si (Silicon)
Li 1980: n 1.2-14 µm; 650 K

Wavelength: µm
 (1.20 – 14.0)  
 

Other optical constants

logX   logY   eV

Comments

650 K (377 °C)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

H. H. Li. Refractive index of silicon and germanium and its wavelength and temperature derivatives, J. Phys. Chem. Ref. Data 9, 561-658 (1993)