Optical constants of Si (Silicon)
Green and Keevers 1995: n 0.25-1.45 µm, k 0.25-1.00 µm

Wavelength: µm
 (0.25 – 1.45)  
 

Other optical constants

n   k   logX   logY   eV

Comments

300 K (27 °C)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

M. A. Green and M. J. Keevers. Optical properties of intrinsic silicon at 300 K, Progress in photovoltaics 3, 189-192 (1995)

More info - wiki

Silicon, Si

Other names for Polysilicon

Polycrystalline silicon; semicrystalline silicon; or simply poly in context

External links