RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of Si (Silicon)
Chandler-Horowitz and Amirtharaj 2005: n 2.5-22.222 µm, k 6.25-23.256 µm

Wavelength: µm
 (2.5 – 23.2558140)  
 

Other optical constants

n   k   logX   logY   eV

Dispersion formula [ i ]

$$n^2=11.67316+\frac{1}{λ^2}+\frac{0.004482633}{λ^2-1.108205^{2}}$$

Comments

Room temperatue.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. Chandler-Horowitz and P. M. Amirtharaj. High-accuracy, midinfrared (450 cm−1 ≤ ω ≤ 4000 cm−1) refractive index values of silicon, J. Appl. Phys. 97, 123526 (2005)