Aspnes and Studna 1983: n,k 0.21-0.83 µm

Wavelength: µm
 (0.2066 – 0.8266)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Crysal orientation: <111>; Doping: 2.3×1014 cm-3, n; Room temperature

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. E. Aspnes and A. A. Studna. Dielectric functions and optical parameters of Si, Ge, GaP, GaAs, GaSb, InP, InAs, and InSb from 1.5 to 6.0 eV, Phys. Rev. B 27, 985-1009 (1983)

More info - wiki

Silicon, Si