RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of Rh (Rhodium)
Windt et al. 1988: n,k 0.0024-0.1216 µm

Wavelength: µm
 (0.00236 – 0.12157)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. L. Windt et al.. Optical constants for thin films of Ti, Zr, Nb, Mo, Ru, Rh, Pd, Ag, Hf, Ta, W, Re, Ir, Os, Pt, and Au from 24 Å to 1216 Å, Appl. Opt. 27, 246-278 (1988)

More info - wiki

Rhodium, Rh

External links