RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of Ni (Nickel)
Ordal et al. 1987: n,k 0.667-286 µm

Wavelength: µm
 (0.667 – 286)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

M. A. Ordal, R. J. Bell, R. W. Alexander, L. L. Long, M. R. Querry. Optical properties of Au, Ni, and Pb at submillimeter wavelengths, Appl. Opt. 26, 744-752 (1987)

More info - wiki

Nickel, Ni

External links