Optical constants of Na (Sodium)
Inagaki et al. 1976: n,k 0.326-2.066 µm

Wavelength: µm
 (0.326 – 2.066)  
 

Other optical constants

n   k   logX   logY   eV

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

T. Inagaki et al. Optical properties of solid Na and Li between 0.6 and 3.8 eV, Phs. Rev. B 13, 2305-2313 (1976)