RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of MoS2 (Molybdenum disulfide)
Yim et al. 2014: 3.01-µm film; n 0.38-0.9 µm

Wavelength: µm
 (0.382127 – 0.888102)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Thickness 3.01 µm

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

C. Yim, M. O'Brien, N. McEvoy, S. Winters, I. Mirza, J. G. Lunney and G. S. Duesberg. Investigation of the optical properties of MoS2 thin films using spectroscopic ellipsometry, Appl. Phys. Let. 104, 103114 (2014)

More info - wiki

Molybdenum disulfide, MoS2

External links