RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of MoO3 (Molybdenum trioxide)
Lajaunie et al. 2013: n(β),k(β) 0.019-24.8 µm

Wavelength: µm
 (1.90745E-2 – 2.47968E+1)  
 

Other optical constants

n   k   logX   logY   eV

Comments

α-MoO3; nβ, kβ.

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

L. Lajaunie, F. Boucher, R. Dessapt, and P. Moreau. Strong anisotropic influence of local-field effects on the dielectric response of α-MoO3, Phys. Rev. B 88, 115141 (2013)
(using numerical data made publically available by Luc Lajaunie)

More info - wiki

Molybdenum trioxide, MoO3

Other names

Molybdic anhydride, Molybdite, Molybdic trioxide, Molybdenum(VI) oxide

External links