RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of MgF2 (Magnesium fluoride)
Dodge 1984: n(o) 0.2-7.0 µm

Wavelength: µm
 (0.2 – 7)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{0.48755108λ^2}{λ^2-0.04338408^2}+\frac{0.39875031λ^2}{λ^2-0.09461442^2}+\frac{2.3120353λ^2}{λ^2-23.793604^2}$$

Comments

19 °C. Ordinary ray (o).

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

M. J. Dodge. Refractive properties of magnesium fluoride, Appl. Opt. 23, 1980-1985 (1984)

More info - wiki

Magnesium fluoride, MgF2

Other names

Magnesium difluoride, Magnesium(II) fluoride

External links