Medenbach et al. 2001: n 0.435-0.644 µm

Wavelength: µm
 (0.435 – 0.644)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{2.609λ^2}{λ^2-0.01722}$$

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

O. Medenbach, D. Dettmar, R. D. Shannon, R. X. Fischer, and W. M. Yen, Refractive index and optical dispersion of rare earth oxides using a small-prism technique, J. Opt. A: Pure Appl. Opt. 3, 174-177, 2001

More info - wiki

Lutetium sesquioxide, Lu2O3

Other names

Lutetium(III) oxide, Dilutetium trioxide, Lutetium oxide.