Optical constants of LiNbO3 (Lithium niobate)
Zelmon et al. 1997: n(o) 0.4-5.0 µm

Wavelength: µm
 (0.4 – 5)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{2.6734λ^2}{λ^2-0.01764}+\frac{1.2290λ^2}{λ^2-0.05914}+\frac{12.614λ^2}{λ^2-474.60}$$

Comments

21 °C. Ordinary ray (o). Congruently grown lithium niobate.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

D. E. Zelmon, D. L. Small, and D. Jundt. Infrared corrected Sellmeier coefficients for congruently grown lithium niobate and 5 mol.% magnesium oxide-doped lithium niobate, J. Opt. Soc. Am. B 14, 3319-3322 (1997)