RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of LiB3O5 (Lithium triborate, LBO)
Chen et al. 1989: n(γ) 0.2894-1.064 µm

Wavelength: µm
 (0.2894 – 1.064)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2=2.58488+\frac{0.012737}{λ^2-0.021414}-0.016293λ^{2}$$

Comments

nγ; Room temperature.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

1) C Chen et al.. New nonlinear-optical crystal: LiB3O5, J Opt. Soc. Am. 6, 616-621 (1989)
2) F. Hanson and D. Dick. Blue parametric generation from temperature-tuned LiB3O5, Opt. Lett. 16, 205-207 (1991).
* Ref. 2 provides Sellmeier equations based on the experimental data from Ref. 1

More info - wiki

Lithium triborate, LiB3O5 (LBO)

External links