Optical constants of LaF3 (Lanthanum fluoride)
Laihoa and Lakkistoa 1983: n(o) 0.35-0.70 µm

Wavelength: µm
 (0.35 – 0.7)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.5376λ^2}{λ^2-0.0881^2}$$

Comments

Ordinary ray (o)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

R. Laihoa and M. Lakkistoa. Investigation of the refractive indices of LaF3, CeF3, PrF3 and NdF3, Phil. Mag. B 48, 203-207 (1983) (As cited in Handbook of Optics, 2nd edition, Vol. 2. McGraw-Hill 1994).