Optical constants of KTiOPO4 (Potassium titanyl phosphate, KTP)
Kato and Takaoka 2002: n(γ) 0.43-3.54 µm

Wavelength: µm
 (0.43 – 3.54)  
 

Other optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2=4.59423+\frac{0.06206}{λ^2-0.04763}+\frac{110.80672}{λ^2-86.12171}$$

Comments

nγ; 20 °C.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

K. Kato and E. Takaoka. Sellmeier and thermo-optic dispersion formulas for KTP, Appl. Opt. 41, 5040-5044 (2002).