RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of In (Indium)
Golovashkin et al. 1967: n,k 0.55-10 µm; 295 K

Wavelength: µm
 (0.55 – 10)  
 

Other optical constants

n   k   logX   logY   eV

Comments

295 K (22 °C)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

A. I. Golovashkin, I. S. Levchenko, G. P. Motulevich, A .A. Shubin. The optical properties of niobium, Sov. Phys. JETP 24, 1093-1099 (1967)

More info - wiki

Indium, In

External links