Optical constants of Ge (Germanium)
Li 1980: n 1.9-18 µm; 250 K

Wavelength: µm
 (1.90 – 18.0)  
 

Other optical constants

logX   logY   eV

Comments

250 K (-23 °C)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

H. H. Li. Refractive index of silicon and germanium and its wavelength and temperature derivatives, J. Phys. Chem. Ref. Data 9, 561-658 (1993)